Thermal and Mechanical Behaviors of Concrete with Incorporation of Strontium-Based Phase Change Material (PCM)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Thermal and Mechanical Behaviors of Concrete with Incorporation of Strontium-Based Phase Change Material (PCM)

Author(s): Hyun-Do Yun1, Kyung-Lim Ahn1, Seok-Joon Jang, Bae-Su Khil, Wan-Shin Park and Sun-Woo Kim

Publication: IJCSM

Volume: 13

Issue:

Appears on pages(s):

Keywords: phase change material, mass concrete, strength development, heat of hydration, adiabatic temperature rise

DOI: 10.1186/s40069-018-0326-8

Date: 3/31/2019

Abstract:
In this study, phase change material (PCM) was used to control the heat of hydration of mass concrete, and the study aimed to evaluate the resulting fundamental and thermal properties of mass concrete with PCM. To evaluate the feasibility of adding PCM to concrete with various binder conditions for mitigating the hydration heat of mass concrete, mechanical and adiabatic temperature rise tests were conducted. The test results showed that the use of PCM did not significantly influence air content, while it slightly reduced flowability. For initial setting properties of concrete, it was found that the initial and final time were delayed when PCM was added. Even though compressive strength was slightly reduced when PCM was added into concrete, the strength development properties of concrete were more closely associated with the strength development properties of the binder. The adiabatic temperature rise test results showed that the addition of PCM resulted in an approximately 15–21% decrease in temperature rise of concrete. From the thermal analysis results, it is noted that thermal cracking probability could be decreased by adding PCM into concrete mix.




  