Title: Effect of High Strain Rates of Reinforced Concrete Bond

Author(s): Eric Jacques

Publication: Web Session

Volume: ws_F18_Jacques.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/15/2018

Abstract:
This presentation will highlight recent research on the effect of high strain rates on the bond strength of reinforcing steel and concrete. To evaluate dynamic bond characteristics, lap spliced reinforced concrete beams were constructed and subjected to blast loading using a shock tube. The physical and material properties of the spliced beams were selected based on a range of design parameters known to significantly influence bond strength (i.e., size of spliced reinforcement, cover depth, concrete strength, and presence of transverse reinforcement). Results of the experiments demonstrated that although the underlying flexural response and nature of bond splitting failure was not affected by dynamic loads, the strength and stiffness of the splices was significantly improved. Without exception, high strain rate bond strength was always greater than corresponding low strain rate values, yielding an average dynamic increase factor (DIF) applied to bond of 1.28. A descriptive expression for the dynamic bond strength of reinforced concrete was developed to account for the observed strain rate sensitivity of splice strength based on member and material properties. Finally, the implications of this research on the design and assessment of structures subjected to blast loads will be discussed.




  

Edit Module Settings to define Page Content Reviewer