Development of a Photovoltaic Integrated Insulated Concrete Sandwich Panel

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Development of a Photovoltaic Integrated Insulated Concrete Sandwich Panel

Author(s): Mostafa Yossef, An Chen and Austin Downey

Publication: Symposium Paper

Volume: 327

Issue:

Appears on pages(s): 29.1-29.18

Keywords: Photovoltaic (PV) integrated insulated concrete sandwich (PVICS) panel; experimental investigation; Finite Element model; analytical solution.

DOI: 10.14359/51713350

Date: 11/1/2018

Abstract:
Insulated concrete sandwich panels are composed of two concrete wythes separated by an insulation layer and connected by shear connectors. This paper develops a multifunctional photovoltaic (PV) integrated insulated concrete sandwich (PVICS) panel, which can act as a passive energy system through the insulation layer and an active energy system by harvesting the solar energy using attached thin-film solar cells. The panel features an innovative co-curing scheme, where solar cells, Fiber-Reinforced Polymer (FRP) shell, and polymer concrete are manufactured together to act as a formwork for the sandwich panel. The objective of this paper is to prove the concept of PVICS based on bending test, Finite Element (FE) analysis and analytical study. It can be concluded that the test results correlate well with those from the FE and analytical models. FRP shell can act as both shear connectors and reinforcement. The panel achieved 82% Degree of Composite Action, which can provide enough strength and stiffness. Solar cells worked properly under service load. Shear-lag effect was observed for the strains along the width of the panel.

Related References:

ABAQUS. (2013). “ABAQUS Documentation.” Dassault Systèmes, Providence, RI, USA.

ACI. (2014). Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14). ACI 318-14.

Benayoune, A., Abdul Samad, A. A., Trikha, D. N., Abang Ali, A. A., and Ellinna, S. H. M. (2008). “Flexural behaviour of pre-cast concrete sandwich composite panel - Experimental and theoretical investigations.” Construction and Building Materials, 22(4), 580–592.

Bush, T. D., and Wu, Z. (1998). “Flexural analysis of prestressed concrete sandwich panels with truss connectors.” PCI journal, Precast/Prestressed Concrete Institute, 43(5), 76–86.

Chen, A., Norris, T. G., Hopkins, P. M., and Yossef, M. (2015). “Experimental investigation and finite element analysis of flexural behavior of insulated concrete sandwich panels with FRP plate shear connectors.” Engineering Structures, 98, 95–108.

Cho, J. R., Cho, K., Park, S. Y., Kim, S. T., and Kim, B. S. (2010). “Bond characteristics of coarse sand coated interface between stay-in-place fibre-reinforced polymer formwork and concrete based on shear and tension tests.” Canadian Journal of Civil Engineering, 37, 706–718.

Einea, A., Salmon, D. C., Fogarasi, G. J., Culp, T. D., and Tadros, M. K. (1991). “State-of-the-Art of Precast Concrete Sandwich Panels.” PCI Journal, 36(6), 78–98.

Einea, A., Salmon, D. C., Tadros, M. K., and Culp, T. (1994). “A New Structurally and Thermally Efficient Precast Sandwich Panel System.” PCI Journal (Precast/Prestressed Concrete Institute), 39(4), 90–101.

Frankl, B. A., Lucier, G. W., Hassan, T. K., and Rizkalla, S. H. (2011). “Behavior of precast, prestressed concrete sandwich wall panels reinforced with CFRP shear grid.” PCI journal, Precast/Prestressed Concrete Institute, 56(2), 42–54.

Fu, R., Feldman, D., Margolis, R., Woodhouse, M., and Ardani, K. (2017). "U.S. Solar Photovoltaic System

Cost Benchmark: Q1 2017 ." National Renewable Energy Laboratory (NREL) Technical Report NREL/TP-6A20-68925. https://www.nrel.gov/docs/fy17osti/68925.pdf

Henin, E., Morcous, G.,, and Tadros, M. K. (2011). “Precast concrete sandwich panels for floor and roof applications.” PCI/NBC, Intergovernmental Panel on Climate Change, ed., Cambridge University Press, Cambridge, 1–30.

Norris, T. G., and Chen, A. (2016). “Development of insulated FRP-confined Precast Concrete Sandwich panel with side and top confining plates and dry bond.” Composite Structures, Elsevier Ltd, 152, 444–454.

Petersen, M.R., Chen, A., Roll, M., Jung, S.J. and Yossef, M. (2015). “Mechanical properties of fire-retardant glass fiber-reinforced polymer materials with alumina tri-hydrate filler,” Composites Part B: Engineering, 78, pp. 109-121.

Petersen, M.R., Yossef, M. and Chen, A.* (2017). “Gap between Code Requirements and Current State of Research on Safety Performance of Fiber-Reinforced Polymer for Non-structural Building Components,” Practice Periodical on Structural Design and Construction, ASCE, 22(4).

Sugar, J. G. (2007). “Photovoltaic Performance of Amorphous Silicon Flexible Solar Modules Under Mechanical Loading.” UCLA.

Yossef, M. (2017). “Development of a multifunctional photovoltaic integrated insulated concrete sandwich panel” PhD Dissertation, Iowa State University, Ames, Iowa, USA.