Title: Strengthening Short Concrete Columns Using Longitudinally Bonded CFRP Laminates

Author(s): Koosha Khorramian and Pedram Sadeghian

Publication: Symposium Paper

Volume: 327

Issue:

Appears on pages(s): 24.1-24.14

Keywords: column, concrete, bonded, CFRP laminate, buckling, BFRP wrap, experimental.

DOI: 10.14359/51713345

Date: 11/1/2018

Abstract:
This paper investigates the behavior of short concrete columns strengthened with externally bonded longitudinal carbon fiber-reinforced polymer (CFRP) laminates combined with transverse basalt fiber-reinforced polymer (BFRP) wraps. A total of eighteen 500 mm-long [19.69 in-long] concrete column specimens with a square cross section (150 mm [5.91 in] width) were tested with different longitudinal and transverse reinforcement combinations under concentric and eccentric axial loadings. For eccentric loading, three end eccentricity to width ratios of 0.1, 0.2, and 0.3 were applied symmetrically at both ends of each simply supported column specimen to provide single curvature condition. The compressive longitudinal CFRP strips, in average, experienced 38% of their tensile rupture strain. The experimental results showed debonding of longitudinal CFRP laminates from concrete surface and buckling of bonded specimens as the dominant mode of failure, and revealed that transverse wrapping system is efficient in postponing the buckling/debonding failure.

Related References:

1. T. C. Triantafillou and N. Plevris, "Strengthening of RC beams with epoxy-bonded fibre-composite materials," Materials and Structures, vol. 25, pp. 201-211, 1992.

2. A. Sharif, G. J. Al-Sulaimani, I. A. Basunbul, M. H. Baluch and B. N. Ghaleb, "Strengthening of Initially Loaded Reinforced Concrete Beams Using FRP Plates," ACI structural Journal, vol. 91, no. 2, pp. 160-168, 1994.

3. H. Rahimi and A. Hutchinson, "Concrete Beams Strengthened with Externally Bonded FRP Plates," Journal of Composites for Construction, vol. 5, no. 1, pp. 44-56, 2001.

4. A. S. Mosallam and K. M. Mosalam, "Strengthening of two-way concrete slabs with FRP composite laminates," Construction and Building Materials, vol. 17, no. 1, pp. 43-54, 2003.

5. Y. J. Kim , J. M. Longworth and G. R. Wight, "Flexure of Two-Way Slabs Strengthened with Prestressed or Nonprestressed CFRP Sheets," Journal of Composites for Construction, vol. 12, no. 4, pp. 366-374, 2008.

6. T. Alkhrdaji, A. Nanni, G. Chen and M. Barker, "Upgrading the Transportation Infrastructure: Solid RC Decks Strengthened with FRP," Concrete International: Design and Construction, vol. 21, no. 10, pp. 37-41, 1999.

7. H. Tarek and S. Rizkalla, "Flexural Strengthening of Prestressed Bridge Slabs with FRP systems," PCI Journal, vol. 47, no. 1, pp. 76-93, 2002.

8. R. Atadero, L. Lee and V. M. Karbhari, "Consideration of material variability in reliability analysis of FRP strengthened bridge decks," Composite Structures, vol. 70, no. 4, pp. 430-443, 2005.

9. M. Shahawy, A. Mirmiran and T. Beitelman, "Tests and modeling of carbon-wrapped concrete columns," Composites Part B: Engineering, vol. 31, no. 6, pp. 471-480, 2000.

10. M. E. Hussein, Y. A. Al-Salloum, S. H. Alsayed and R. A. Iqbal, "Experimental and numerical investigation of size effects in FRP-wrapped concrete columns," Construction and Building Materials, vol. 29, pp. 56-72, 2012.

11. A. Mirmiran, M. Shahawy, M. Samaan, H. El Echary, J. C. Mastrapa and O. Pico, "Effect of Column Parameters on FRP-Confined Concrete," Journal of Composites for Construction, vol. 2, no. 4, pp. 175-185, 1998.

12. D. A. Bournas and T. C. Triantafillou, "Flexural strengthening of reinforced concrete columns with near-surface-mounted FRP or stainless steel," ACI Structural Journal, vol. 106, no. 4, pp. 495-505, 2009.

13. K. Gajdosova and J. Bilcik, "Full-Scale Testing of CFRP-Strengthened Slender Reinforced Concrete Columns," Journal of Composites for Construction, vol. 17, no. 2, pp. 239-248, 2013.

14. A. Parvin and W. Wang, "Behaviour of FRP jacketed concrete columns under eccentric loading," Journal of Composites for Construction, vol. 5, no. 3, pp. 146-152, 2001.

15. M. N. S. Hadi, "Behaviour of FRP wrapped normal strength concrete columns under eccentric loading," Composite Structures, vol. 72, no. 4, pp. 503-511, 2006.

16. L. Bisby and M. Ranger, "Axial–flexural interaction in circular FRP-confined reinforced concrete columns," Construction and Building Materials, vol. 24, no. 9, pp. 1672-1681, 2010.

17. A. Parvin and D. Brighton, "FRP Composites Strengthening of Concrete Columns under various loading conditions," Polymers, vol. 6, pp. 1040-1056, 2014.

18. P. Sadeghian and A. Fam, "Strengthening Slender Reinforced Concrete Columns Using High-Modulus Bonded Longitudinal Reinforcement for Buckling Control," Journal of Structural Engineering, vol. 141, no. 4, p. 04014127, 2015.

19. A. Shaat and A. Z. Fam, "Slender Steel Columns Strengthened Using High-Modulus CFRP Plates for Buckling Control," Journal of Composites for Construction, vol. 13, no. 1, pp. 2-12, 2009.

20. O. Chaallal and M. Shahawy, "Performance of Fiber-Reinforced Polymer-Wrapped Reinforced Concrete Column under Combined Axial-Flexural Loading," ACI Structural Journal, vol. 97, no. 4, pp. 659-668, 2000.

21. P. Sadeghian, A. R. Rahai and M. R. Ehsani, "Experimental Study of Rectangular RC Columns Strengthened with CFRP Composites under Eccentric Loading," Journal of Composites for Construction, vol. 14, no. 4, pp. 443-450, 2010.

22. T. M. Pham, J. Youssed, M. N. Hadi and T. M. Tung, "Effect of Different FRP Wrapping Arrangements on the Confinement Mechanism," Procedia Engineering, vol. 142, pp. 307-313, 2016.

23. ASTM D3039/D3039M-14, Standard Test Method for Tensile Properties of Polymer Matrix Composite Materials, West Conshohocken, PA: American Society for Testing and Materials, 2014.

24. B. Fillmore and P. Sadeghian, "Strain Distribution of Basalt FRP-Wrapped Concrete Cylinders," Work-in-progress, 2017.

25. ACI 318-14, Building Code Requirements for Structural Concrete, Farmington Hills, MI: American Concrete Institute, 2014.