International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: An Analytical Model to Predict Flexural Behavior of NSM FRP-Strengthened RC Beams Subject to Debonding Failure

Author(s): Cheng Chen and Lijuan Cheng

Publication: Symposium Paper

Volume: 327

Issue:

Appears on pages(s): 7.1-7.24

Keywords: Fiber reinforced polymer (FRP); near-surface mounted (NSM); flexural; concrete; debonding

DOI: 10.14359/51713327

Date: 11/1/2018

Abstract:
An analytical model is proposed in this study to predict the flexural behavior of reinforced concrete (RC) beams strengthened with near-surface mounted (NSM) fiber reinforced polymer (FRP) reinforcements due to debonding failure. In modeling the RC beam-NSM FRP system, a trilinear bond-slip relation is adopted for the interfacial stress between the two components. A closed-form solution is obtained by imposing appropriate boundary conditions for bond stress, FRP strain and deflection of the strengthened beams. The results are verified by the comparison with experimental data from different studies, where satisfactory correlation is obtained such as flexural deflection and tensile strain of FRP reinforcement. A parametric study is further conducted, which shows that the diameter of the FRP reinforcement and the steel rebar significantly affects the flexural performance of the NSM-strengthened RC beams. The Young’s modulus, the compressive strength of concrete and the bond strength of FRP reinforcement improve the performance to a lesser extent.




  