Effect of GFRP compression reinforcement on long-term deflections

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of GFRP compression reinforcement on long-term deflections

Author(s): Stephanie L. Walkup, Eric S. Musselman, and Shawn P. Gross

Publication: Symposium Paper

Volume: 327

Issue:

Appears on pages(s): 6.1-6.20

Keywords: compression reinforcement; long-term deflection; FRP reinforced beams; beam deflection; deflection multiplier; GFRP reinforced beams

DOI: 10.14359/51713326

Date: 11/1/2018

Abstract:
The effect of compression reinforcement to reduce long term deflections in GFRP-reinforced concrete beams was evaluated. Nine GFRP-reinforced specimens and three companion steel-reinforced specimens were tested under sustained load for a period of 100 days. Long-term deflection data was used to evaluate the reduction in long-term multiplier for GFRP-reinforced beams and the effects of the compression reinforcement to further reduce the multiplier. Compression reinforcement reduced the long-term multiplier for the GFRP- and steel-reinforced specimens. A new equation is proposed to incorporate the compression reinforcement index, kr, in the long-term deflection multiplier for any type of reinforcement. The experimental results also demonstrate that the ratio of the long-term deflection of a GFRP-reinforced vs. steel-reinforced beam can be determined in a relatively short period of time. Experimental results from the present study show that this ratio is 0.87 for the GFRP-reinforced specimens without compression reinforcement, in lieu of the present 0.6 value used in ACI 440.1R. Keywords:

Related References:

1. ACI Committee 318 (2014), “Building Code Requirements for Reinforced Concrete and Commentary,” ACI 318-14/ACI 318R-14, American Concrete Institute, Farmington Hills, Michigan, 430 p.

2. ACI Committee 440, (2015), “Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer (FRP) Bars,” ACI 440.1R-15, American Concrete Institute, Farmington Hills, Michigan, 88 p.

3. Arockiasamy, M., Amer, A., and Shahawy, M, (1998), “Environmental and long-term studies of CFRP cables and CFRP reinforced concrete beams,” Proceedings of the First International Conference on Durability of Composites for Construction, Sherbrooke, Quebec, Canada, August, pp.599-610.

4. Branson, D. E., (1977), “Deformation of Concrete Structures,” McGraw Hill, New York, 546 p.

5. Brown., V., (1997), “Sustained Load Deflections in GFRP-Reinforced Concrete Beams,” Non-Metallic (FRP) Reinforcement for Concrete Structures (FRPRCS-3), Proceedings of the 3rd International Symposium on Nonmetallic (FRP) Reinforcement for Concrete Structures, Sapporo, Japan, October 14-16, Vol. 2, pp. 495-502.

6. Gross, S.P., Yost, J., and Kevgas, G., (2003), “Time-Dependent Behavior of Normal and High Strength Concrete Beams Reinforced with GFRP Bars Under Sustained Load,” High Performance Materials in Bridges, American Society of Civil Engineers, pp.451-462.

7. Gross, S.P., Yost, J.R., and Crawford, J., (2006), “Serviceability of High Strength Concrete Beams with Internal FRP Reinforcement under Sustained Load,” Proceedings of the Third International Conference on FRP Composites in Civil Engineering (CICE 2006), Miami, Florida, USA, December 13-15, pp.203-206.

8. Hall, T., and Ghali, A., (2000), “Long-Term Deflection Prediction of Concrete Members Reinforced with Glass Fiber Reinforced Polymer Bars,” Canadian Journal of Civil Engineering, Ottawa, Ontario, Canada, 27: 890-898.

9. Hollington, M.R., (1970), “A Series of Long-Term Tests to Investigate the Deflection of a Representative Precast Concrete Floor Component,” Technical Report TRA 442, Cement and Concrete Association, London, 43 p.

10. Kage, T., Masuda, Y., Tanano, Y., and Sato, K., (1995), “Long-term Deflections of Continuous Fiber Reinforced Concrete Beams,” Proceedings of the Second International Symposium on Non-Metallic (FRP) Reinforcement for Concrete Structures (FRPRCS-2), Ghent, Belgium, October 23-25, pp.251-258.

11. Laoubi, K., El-Salakawy, E., and Benmokrane, B., (2006), “Behavior of Concrete Beams Reinforced with GFRP Bars under Sustained Load and Freeze/Thaw Cycles,” Proceedings of the 2nd International Conference on Durability of Fibre Reinforced Polymer (FRP) Composites for Construction, Sherbrooke, Quebec, Canada, pp.453-464.

12. Mias, C., Torres, L., Turon., A., Barris, C., (2013a), “Experimental Study of Immediate and Time-Dependent Deflections of GFRP Reinforced Concrete Beams,” Composite Structures, Vol. 96, pp. 279-285.

13. Mias, C., Torres, L., Turon, A., and Sharaky, I., (2013b), “Effect of Material Properties on Long-Term Deflection of GFRP Reinforced Concrete Beams,” Construction and Building Material, Vol. 41, pp. 99-108.

14. Nanni, A., DeLuca, A., Zadeh, H., “Reinforced Concrete with FRP Bars: Mechanics and Design,” CRC Press, Boca Raton, Florida, 2014, 418p.

15. Shaikh, A.F., and Branson, D.E., (1970), “Non-tensioned Steel in Prestressed Concrete Beams,” PCI Journal, Vol. 15, No. 1, pp.14-36.

16. Vijay, P., and GangaRao, H., (1998), “Creep Behavior of Concrete Beams Reinforced with GFRP Bars,” Proceedings of the First International Conference on Durability of Composites for Construction (CDCC’98),” Sherbrooke, Quebec, Canada, August pp.661-667.

17. Wang, Z., Goto, Y., Joh, O. (1997), “Bond Characteristics of FRP Rods and Effect on Long Term Deflection of Concrete Beams,” Non-Metallic (FRP) Reinforcement for Concrete Structures (FRPRCS-3), Proceedings of the 3rd International Symposium on Nonmetallic (FRP) Reinforcement for Concrete Structures, Sapporo, Japan, October 14-16, Vol. 2, pp. 389-396.

18. Washa, G.W., and Fluck, P.G., (1952), “Effect of compressive reinforcement on the plastic flow of reinforced concrete beams,” ACI Journal, 24(2), (Proceedings Vol. 49), pp. 89-108.

19. Washa, G.W., and Fluck, P.G., (1956), “Effect of compressive reinforcement on the plastic flow of reinforced concrete continuous beams,” ACI Journal, 27(5), (Proceedings Vol. 52), pp. 549-562.

20. Youssef, T, El-Gamal, S., Benmokrane, B., (2009a), “Long-term deflection of GFRP-reinforced concrete beams under uniform sustained load,” 1st International /1st Engineering Mechanics and Materials Specialty Conference, St. John’s, Newfoundland and Labrador, May 27-30, 9 p.

21. Youssef, T., El-Gamal, S., El-Salakawy, E., and Benmokrane, B., (2009b), “Deflection and Strain Variation of GFRP-Reinforced Concrete Beams after One Year of Continuous Loading,” 9th International Symposium on Fiber Reinforced Polymer Reinforcement for Concrete Structures, Sydney, Australia, July 13-15, 4 p.

22. Yu, W.W., and Winter, G., (1960), “Instantaneous and Long-Time Deflections of Reinforced Concrete Beams Under Working Loads,” ACI Journal 57(2), pp. 29-50.

23. Zawam, M., (2015), “Long-Term Behaviour of GFRP Prestressed Concrete Beams” Doctorate Thesis, University of Waterloo, 182 p.