Rheological Properties of Cement Pastes Incorporating Polycarboxylate Superplasticizers Containing Different Hydrophobic Groups

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Rheological Properties of Cement Pastes Incorporating Polycarboxylate Superplasticizers Containing Different Hydrophobic Groups

Author(s): Xin Shu, Yanwei Wang, Yong Yang, Xiumei Wang, Qian Zhang, Hongxia Zhao, Qianping Ran, and Jiaping Liu

Publication: Symposium Paper

Volume: 329

Issue:

Appears on pages(s): 333-348

Keywords: yield stress; apparent viscosity; cement paste; hydrophobic; stiffness

DOI: 10.14359/51711225

Date: 9/26/2018

Abstract:
Rheological properties of cement pastes with polycarboxylate superplasticizers (PCE) containing different hydrophobic groups (styrene, n-butyl acrylate units) at different water to cement ratios (w/c) were investigated. Further investigation on the solution behavior (hydrodynamic radius, solution viscosity) and adsorption behavior revealed the fundamental difference of these PCE samples. At high w/c, the rheological properties of cement pastes primarily depended on the ALT and the differences at constant flow diameter were small. At low w/c, the yield stress primarily depended on the ALT, while the apparent viscosity difference relied on the balance of ALT and solution viscosity. The styrene unit enhanced the backbone stiffness and therefore the adsorption affinity, intrinsic viscosity, yet smaller ALT, therefore reduced the apparent viscosity at a proper dosage. The n-butyl acrylate unit always increased the apparent viscosity of cement pastes.

Related References:

1. Yamada, K.; Takahashi, T.; Hanehara, S.; and Matsuhisa, M., “Effects of the chemical structure on the properties of polycarboxylate-type superplasticizer,” Cement and Concrete Research, V. 30, No. 2, 2000, pp. 197-207. doi: 10.1016/S0008-8846(99)00230-6

2. Sakai, E.; Yamada, K.; and Ohta, A., “Molecular structure and dispersion-adsorption mechanisms of comb-like superplasticizers used in Japan,” Journal of Advanced Concrete Technology, V. 1, No. 1, 2003, pp. 16-25. doi: 10.3151/jact.1.16

3. Giraudeau, C.; d’Espinose de Lacaillerie, J.-B.; Souguir, Z.; Nonat, A.; and Flatt, R. J., “Lacaillerie J-B d’E, Souguir Z, Nonat A, and Flatt RJ., “Surface and intercalation chemistry of polycarboxylate copolymers in cementitious systems,” Journal of the American Ceramic Society, V. 92, No. 11, 2009, pp. 2471-2488. doi: 10.1111/j.1551-2916.2009.03413.x

4. Plank, J.; Sakai, E.; Miao, C. W.; Yu, C.; and Hong, J. X., “Chemical admixtures — Chemistry, applications and their impact on concrete microstructure and durability,” Cement and Concrete Research, V. 78, December, 2015, pp. 81-99. doi: 10.1016/j.cemconres.2015.05.016

5. Phan, T. H.; Chaouche, M.; and Moranville, M., “Influence of organic admixtures on the rheological behaviour of cement pastes,” Cement and Concrete Research, V. 36, No. 10, 2006, pp. 1807-1813. doi: 10.1016/j.cemconres.2006.05.028

6. Papo, A., and Piani, L., “Effect of various superplasticizers on the rheological properties of Portland cement pastes,” Cement and Concrete Research, V. 34, No. 11, 2004, pp. 2097-2101. doi: 10.1016/j.cemconres.2004.03.017

7. Banfill, P. F. G., “Additivity effects in the rheology of fresh concrete containing water-reducing admixtures,” Construction & Building Materials, V. 25, No. 6, 2011, pp. 2955-2960. doi: 10.1016/j.conbuildmat.2010.12.001

8. Kwan, A. K. H., and Fung, W. W. S., “Role of water film thickness in rheology of CSF mortar,” Cement and Concrete Composites, V. 32, No. 4, 2010, pp. 255-264. doi: 10.1016/j.cemconcomp.2010.01.005

9. Kwan, AKH., and Fung, WWS., “Roles of water film thickness and SP dosage in rheology and cohesiveness of mortar,” Cement and Concrete Composites, V. 34, No. 2, Feburary 2012, pp. 121-130.

10. Zhang, Q. Q.; Liu, J. Z.; Liu, J. P.; Han, F. Y.; and Lin, W.Effect of Superplasticizers on Apparent Viscosity of Cement-Based Material with a Low Water–Binder Ratio, V. 28, No. 9, September 2016, doi: 10.1061/(ASCE)MT.1943-5533.0001590

11. Hot, J.; Bessaies-Bey, H.; Brumaud, C.; Duc, M.; Castella, C.; and Roussel, N., “Adsorbing polymers and viscosity of cement pastes,” Cement and Concrete Research, V. 63, September, 2014, pp. 12-19. doi: 10.1016/j.cemconres.2014.04.005

12. Shu, X, Zhao, HX., Wang, XM., Zhang, Q., Yang, Y., Ran, QP., and Liu, JP., “Effect of hydrophobic units of polycarboxylate superplasticizer on the flow behavior of cement paste”, Journal of Dispersion Science and Technology, V. 38, No. 2, Feburary 2017, pp. 256-264.

13. Ng, S., and Plank, J., “Interaction mechanisms between Na montmorillonite clay and MPEG-based polycarboxylate superplasticizers,” Cement and Concrete Research, V. 42, No. 6, 2012, pp. 847-854. doi: 10.1016/j.cemconres.2012.03.005

14. Shu, X.; Ran, Q. P.; Liu, J.; Zhao, H. X.; Zhang, Q.; Wang, X. M.; Yang, Y.; and Liu, J. Z., “Tailoring the solution conformation of polycarboxylate superplasticizer toward the improvement of dispersing performance in cement paste,” Construction & Building Materials, V. 116, July, 2016, pp. 289-298. doi: 10.1016/j.conbuildmat.2016.04.127

15. Roussel, N.; Lemaître, A.; Flatt, R. J.; and Coussot, P., “Steady state flow of cement suspensions: a micromechanical state of the art,” Cement and Concrete Research, V. 40, No. 1, 2010, pp. 77-84. doi: 10.1016/j.cemconres.2009.08.026

16. Ran, Q. P.; Somasundaran, P.; Miao, C. W.; Liu, J. P.; Wu, S. S.; and Shen, J., “Effect of the length of the side chains of comb-like copolymer dispersants on dispersion and rheological properties of concentrated cement suspensions,” Journal of Colloid and Interface Science, V. 336, 2, 2009, pp. 624-633. doi: 10.1016/j.jcis.2009.04.057

17. Flatt, RJ., and Bowen, P., “Yodel: a yield stress model for suspensions,” Journal of the American Ceramic Society, V. 89, No. 4, Feburary 2006, pp. 1244-1256.

18. Flatt, R. J., and Bowen, P., “Yield stress of multimodal powder suspensions: an extension of the YODEL (Yield Stress mODEL),” Journal of the American Ceramic Society, V. 90, No. 4, 2007, pp. 1038-1044. doi: 10.1111/j.1551-2916.2007.01595.x

19. Chop, G. N., and Krieger, I. M., “Rheological studies on sterically stabilized dispersions of uniform colloidal spheres: I. Sample Preparation,” Journal of Colloid and Interface Science, V. 113, No. 1, 1986, pp. 94-100. doi: 10.1016/0021-9797(86)90209-2

20. Liu, J. Z.; Wang, K. J.; Zhang, Q. Q.; Han, F. Y.; Sha, J. F.; and Liu, J. P., “Influence of superplasticizer dosage on the viscosity of cement paste with low water-binder ratio,” Construction & Building Materials, V. 149, May, 2017, pp. 359-366. doi: 10.1016/j.conbuildmat.2017.05.145

21. Dalas, F.; Nona, A.; Pourchet, S.; Mosquet, M.; Rinaldi, D.; and Sabio, S., “Tailoring the anionic function and the side chains of comb-like superplasticizers to improve their adsorption,” Cement and Concrete Research, V. 67, January, 2015, pp. 21-30. doi: 10.1016/j.cemconres.2014.07.024

22. Plank, J.; Sachsenhauser, B.; and Reese, J., “Experimental determination of the thermodynamic parameters affecting the adsorption behaviour and dispersion effectiveness of PCE superplasticizers,” Cement and Concrete Research, V. 40, No. 5, 2010, pp. 699-709. doi: 10.1016/j.cemconres.2009.12.002

23. Marchon, D.; Mantellato, S.; Eberhard, A. B.; and Flatt, R. J., “Adsorption of chemical admixtures,” Science and Technology of Concrete Admixtures, Woodhead Publishing Limited, Cambrige, 2016, pp. 226-232.

24. Flatt, R. J.; Schober, I.; Raphael, E.; Plassard, C.; and Lesniewska, E., “Conformation of adsorbed comb copolymer dispersants,” Langmuir, V. 25, No. 2, 2009, pp. 845-855. doi: 10.1021/la801410e

25. Liu, J. P.; Ran, Q. P.; Miao, C. W.; and Qiao, M., “Effects of grafting densities of comb-like copolymer on the dispersion properties of concentrated cement suspensions,” Materials Transactions, V. 53, No. 2, 2012, pp. 553-558. doi: 10.2320/matertrans.M2011344

26. Zhang, Q.; Ran, Q. P.; Zhao, H. X.; Shu, X.; Yang, Y.; Zhou, H. X.; and Liu, J. P., “pH-induced conformational changes of comb-like polycarboxylate investigated by experiment and simulation,” Colloid & Polymer Science, V. 294, No. 11, 2016, pp. 1705-1715. doi: 10.1007/s00396-016-3932-5