Experimental Evaluation of the Efficiency of FRCM-U-Wrap Joist Tech for Flexural Improvement of RC Beam

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Evaluation of the Efficiency of FRCM-U-Wrap Joist Tech for Flexural Improvement of RC Beam

Author(s): Laura Anania

Publication: Symposium Paper

Volume: 326

Issue:

Appears on pages(s): 106.1-106.10

Keywords: composite structures, concrete structures, fiber-reinforced cementitious mortars (FRCM), flexural capacity, strengthening

DOI: 10.14359/51711089

Date: 8/10/2018

Abstract:
The paper reports the results of an experimental investigation aimed to the assessment of the enhancement of the flexural capacity of RC beam. The technology employed is based on the use of Fiber-Reinforced Cementitious Matrix (FRCM). The patented system, called FRCM U-Wrap-Joist Tech provides a new methodology for beam strengthening capable of generating a higher internal couple of the cross section with no incisive change of the element weight. That can be aimed by the employment of a poor weight joist, joined at the intrados of the original beam and connected to the extremities with two reoplastic mortar blocks. The joist was, then, jacked in a FRCM material based on PBO composite net. This produces an increment of the compressed zone of the cross section and it lowers traction stress values in steel as well as compression stress values in concrete. Experimental evidence gives back an increase in flexural strength equal to the double than the original non-reinforced beam, as well as a, considerably, greater than the reinforced beam according to traditional technology where the fiber net is directed glued to the beam intrados. So, this methodology seems to be very useful in the case of a transformation of the use destination of a civil structure when an increase of the resistant section is required and in any case of seismic strengthening intervention.

Related References:

1. American Concrete Institute, “Building code requirements for reinforced concrete” ACI 318, Farmington Hills, MI. (2011)

2. ACI Committee 440. Guide for the design and construction of externally bonded FRP systems for strengthening concrete structures (ACI 440.2R- 08). Farmington Hills, MI: American Concrete Institute; 2008.

3. AC 434 “Acceptance Criteria for Masonry and Concrete Strengthening Using Fiber-Reinforced Cementitious Matrix (FRCM) Composite Systems” Design Manual for Ruredil Icc-Es. (2013).

4. Anania L, Badala A, Failla G (2005). Increasing the flexural performance of RC beams strengthened with CFRP materials. Construction and Building Materials, V. 19, p. 55-61, ISSN: 0950-0618, doi: 10.1016/j.conbuildmat.2004.04.01

5. Di Tommaso A, Focacci F, Mantegazza G, Gatti A. FRCM versus FRP composites to strengthen RC beams: a coMParative analysis. In: Triantafillou TC, editor. Proceedings of the international symposium on fibre reinforced polymers for reinforced concrete structures (FRPRCS8), Patras, Greece; 2007.

6. Di Tommaso A, Focacci F, Mantegazza G. PBO-FRCM composites to strengthen RC beams: mechanics of adhesion and efficiency. In: Motavalli M, editor. Proceedings of the international conference on FRP composites in civil engineering (CICE 2008), Zurich, Switzerland; 2008.

7. Saad M. Raoof, Lampros N. Koutas, Dionysios A. Bournas “Bond between textile-reinforced mortar (TRM) and concrete substrates: Experimental investigation” Composites Part B: Engineering, V. 98, 2016, pp. 350-361

8. Zoi C. Tetta, Lampros N. Koutas, Dionysios A. Bournas “Textile-reinforced mortar (TRM) versus fiber-reinforced polymers (FRP) in shear strengthening of concrete beams” Composites Part B: Engineering Volume 77, August 2015, pp. 338-348

9. Hussein M.Elsanadedy, Tarek H.Almusallam Saleh H.AlsayedYousef A.Al-Salloum “Flexural strengthening of RC beams using textile reinforced mortar – Experimental and numerical study”, Composite Structures, V. 97, March 2013, pp. 40-55

10. Yousef A. Al-Salloum, Hussein M. Elsanadedy, Saleh H. Alsayed and Rizwan A. Iqbal, “Experimental and numerical study for the shear strengthening of reinforced concrete beams using textile-reinforced mortar”, Journal of Composites for Construction, V. 16, Issue 1 ISSN (print): 1090-0268 | ISSN (online): pp. 1943-5614

11. Wobbe E, Silva P, Barton BL, Dharani LR, Birman V, Nanni A, et al. Flexural capacity of R/C beams externally bonded with SRP and SRG. In: Proc of society for the advancement of material and process engineering symp, Long Beach, CA, USA. p. 20–7.

12. Prota A, Manfredi G, Nanni A, Cosenza E, Pecce M. Flexural strengthening of R/C beams using emerging materials: ultimate behavior. In: Proc of CICE, Adelaide, Australia. p. 163–70.

13. Lesley H. Sneed, Salvatore Verre, Christian Carloni, Luciano Ombres- “Flexural behavior of RC beams strengthened with steel-FRCM composite”, Engineering Structures, V. 127, 2016, pp. 686–699

14. Ombres L. “Flexural analysis of reinforced concrete beams strengthened with a cement based high strength composite”, Composite Structures, V. 94, 2011, pp. 143–155

15. Toutanji H, Deng Y. CoMParison between organic and inorganic matrices for RC beams strengthened with carbon fiber sheets. J Compos Constr ASCE 2007, V. 11, No. 5, pp. 507–13.

16. Toutanji H, Zhao L, Zhang Y. Flexural behavior of reinforced concrete beams externally strengthened with CFRP sheets bonded with an inorganic matrix. Eng Struct, Elsevier, V. 28, 2006, pp. 557–66.

17. Ueno, S., Toutanji, H., Vuddandam, R. (2015), “Introduction of Critical Stress State Criterion to Predict Bond Strength between FRP and Concrete Substrate” ASCE Composites for Construction Journal, V. 19, Issue 1, P. 04014024 (1-11).

18. Anania L, D'Agata G. “Numerical validation of Double Punch Test for the assessment of tensile strength in natural fiber reinforced concrete”. Mechanics of Advanced Materials and Structures, ISSN: 1537-6494, doi: 10.1080/15376494.2017.1387328

19. Anania L, Badala A, D'Agata G “Numerical simulation of tests for the evaluation of the performance of the reinforced concrete slabs strengthening by FRCM” Curved and Layered Structures, V. 3, p. 63-73, ISSN: 2353-7396, doi: 10.1515/cls-2016-0005Anania L

20. J.H. Gonzalez-Libreros, L.H. Sneed b, T. D’Antino, C. Pellegrino “Behavior of RC beams strengthened in shear with FRP and FRCM composites”, Engineering Structures, V. 150, 2017, pp. 830–842

21. Pellegrino C, Modena C. “Fiber-reinforced polymer shear strengthening of reinforced concrete beams: experimental study and analytical modeling”. ACI Struct J, V. 103, 2007, pp. 720–8.

22. Chen GM, Teng JG, Chen JF, Rosenboom O. “Interaction between steel stirrups and shear-strengthening FRP strips in RC beams”, J Compos Constr, V. 14, 2010, pp. 498–509

23. DM 2008

24. Comité Européen de Normalisation, EN 12390-1. Testing hardened concrete –Part 1: Shape, dimensions and other requirements for specimens and moulds, (2012).

25. Comité Européen de Normalisation, EN 12390-3. Testing hardened concrete –Part 3: Compressive strength of test specimens, (2009).

26. Comité Européen de Normalisation, EN ISO 15630-1. Steel for the reinforcement and prestressing of concrete. Test methods – Part 1: Reinforcing bars, wire rod and wire, (2010)

27. ACI 549.4R-13 “Design and Construction of Externally Bonded FRCM Systems “American Concrete Institute (2013)

28. ACI 562-13—Code Requirements for Evaluation, Repair, and Rehabilitation of Concrete Buildings and Commentary American Concrete Institute (2013)

29. G Campione, F Cannella, L Cavaleri, “Shear and Flexural Strength Prediction of Corroded R.C. Beams” Construction and Building Materials, V. 149, 2017, pp. 395-405 DOI 10.1016/j.conbuildmat.2017.05.125

30. D. Coronelli, P. Gambarova, “Structural assessment of corroded reinforced concrete beams: modeling guidelines”, ASCE J. Struct. Eng. V. 130, No. 8, 2004, pp. 1214– 1224

31. S. Ting, A. Nowak, “Effect of reinforcing steel area loss on flexural behavior of RC beams”, ACI J. Struct Eng., V. 88, No. 3, 1991, pp. 309–314

32. G.J. Al-Sulaimani, M. Kaleemullah, I.A. Basumbul, Rasheeduzzafar, “Influence of corrosion and cracking on bond behavior and strength of reinforced concrete members”, ACI Struct. J., V. 87, 1991, pp. 220–231

33. D. Coronelli, “Corrosion cracking and bond strength modeling for corroded bars in reinforced concrete”, ACI Struct. J., V. 99, No. 3, 2002, pp. 267–276

34. D. Coronelli, Z.H. Kamyab, K. Lundgren, “Severely corroded RC with cover cracking”, J. Struct. Eng., V. 139, No. 2, 2013, pp. 221–232

35. Anania L, D’agata G. “Innovative technologies in the upgrading of Exiting RC Framed structures Book Title: Earthquake Resistant Engineering Structures X", pp. 159-170 WIT Transactions on The Built Environment, Vol 152, 2015, © 2015 WIT Press ISBN: 978-1-84564-966-1 ISBN: 978-1-84564-967-8 ISSN: 1746-4498 (print) - ISSN: 1743-3509 (on-line)