Title:
Influence of Negative Temperatures on Water Permeability of Concrete
Author(s):
Anatoly Vovk and Irina Vovk
Publication:
Symposium Paper
Volume:
326
Issue:
Appears on pages(s):
85.1-85.8
Keywords:
antifreeze admixtures, microstructure, negative temperatures, ready-mix concrete, water permeability
DOI:
10.14359/51711068
Date:
8/10/2018
Abstract:
In countries with severe climate, in winter period ready-mix concrete is exposed to cooling down during transportation and placing before heat impact. To eliminate negative influence of negative temperatures, antifreeze admixtures are used purposely. Russian Standard GOST 24211-2008 stipulates antifreeze admixtures performance testing both at short negative temperature exposure (so called “warm” concrete) and for permanent hardening at temperatures below zero. In both cases the only performance criteria is concrete compressive strength. On the other side, in European standards such tests are not provided as a rule.
Statistically, nowadays antifreeze admixtures are used in very low dosage (~2÷3% of liquid commercial products for up to -25°С for “cold” concrete and even less for “warm” concrete technology). It was established, that, while using such amount of antifreeze admixtures, even short term exposure to negative temperatures (without concrete freezing) can adversely effects concrete`s water permeability. On examples on set of concretes with different dosages of common antifreeze admixture (up to maximum level recommended by “Temporary Construction Standards” 46-96 for -5÷-15°С range), main factors that influence on water permeability of concretes hardened under negative temperatures were observed. The formation of a fine microstructure due to the pozzolanic additive increases the resistance of the concrete to freezing, but the stability of the concrete water permeability can be achieved only by ensuring near-zero ice formation in the pore liquid.
Related References:
1. GOST 24211-2008. Admixtures for concretes and mortars. General specifications.
2. GOST 30459-2008. Admixtures for concretes and mortars. Determination and estimate of the efficiency.
3. Vovk, A. “Silica fume in concrete technology: new case studies”. ICCM Montreal, Canada, October 2-4, 2017.
4. Evdokimov, N.I., Matskiewich, and A.F., Sytnik, V.S., “Technology of in-situ concrete and reinforced concrete”, Publishing house “Vysshaya Shkola”, Moscow, 1980, 335 pp.
5. Vovk, A. “Blended Antifreezing Admixtures with Extreme Freezing-Point”, Superplasticizers and Other Chemical Admixtures in Concrete, SP-302-21, V.M. Malhotra, ed., American Concrete Institute, Farmington Hills, Mich., 2015, pp. 279-287.
6. GOST 30459-96. Admixtures for concretes. Methods of determining the efficiency.
7. Pashkevich, S.A., Adamtsevich, A.O., Pustovgar, A.P., Golunov, S.A., and Shishiyanu, N.N. “Research of formation of pore structure of cement systems that harden at low and negative temperatures”, Vestnik MGSU. 2012, ?3, pp.120–125.
8. Massoussi, N., Keita, E., and Roussel, N. “The heterogeneous nature of bleeding in cement pastes”, Cement and Concrete Research, V. 95 (2017), pp. 108–116.