Title: Methodology of Long-Term Concrete Tests for Bending

Author(s): Petr Arleninov, Sergey Krylov, and Dmitry Kuzevanov

Publication: Symposium Paper

Volume: 326

Issue:

Appears on pages(s): 78.1-78.6

Keywords: Calculation of structures, concrete, creep, deformations, reinforced concrete, non-liner calculation

DOI: 10.14359/51711061

Date: 8/10/2018

Abstract:
Two main novelties are proposed in this article: the first is an introduction that details deformation characteristics — long-term modulus of concrete elasticity during bending and its differentiation, and the second is the proposed simplified method for creep testing during the bending mode with the further matching of results with classic testing for compression in spring test rigs.

Related References:

1. Sanzharovskii R.S. Musabaev. T.T., 1996. “Elasto-plastic deformation of reinforced concrete covers and plates with cracks”, Izv. vuzov. Ser. Stroitel'stvo i arkhitektura, pp. 3-11. (In Russian).

2. Alexander, M. G., “Aggregates and the Deformation Properties of Concrete”, ACI Materials Journal, Vol. 93(No.6), 1996, pp. 569-577.

3. Haranki B., “Strength, modulus of elasticity, creep and shrinkage of concrete used in Florida”. 2009.

4. Tsilosani Z.N., “Usadka i polzuchest' betona Shrinkage and creep of concrete.”, Izd-vo AN Gruz. SSR, 1963. (In Rusian).

5. SP 63.13330.2012, “Betonnye i zhelezobetonnye konstrukcii. Osnovnye polozhenija Set of Rules. 63.13330.2012. Concrete and reinforced concrete designs. Basic provisions.,” Moscow, 2012. (In Rusian).

6. GOST 24452-80 “Betony. Metody ispytanij State Standart 24452-80. Concrete. Test methods.,” Moscow, Standartinform Publ., 2005. (In Rusian).

7. SP 52-103-2007, “Zhelezobetonnye monolitnye konstrukcii zdanij Set of Rules. 63.13330.2012. Reinforced concrete monolithic structures of buildings.,” Moscow, 207. (In Rusian).

8. ?rylov S.B., “Arleninov P.D., The core bend equation at the piecewise and linear law of deformation of creeping material”. Stroitel'naja mehanika i raschet sooruzhenij. ?3, 2013, pp. 6-9. (In Russian).

9. Arleninov P.D., “Deformation and stability of compressed is also non-central the compressed rod reinforced concrete elements taking into account creep and a treshchinoobrazovaniye”, Cand. diss. (Engineering). Moscow. Niizhb named A.A. Gvozdev, 2016, 143 p. (In Russian).

10. Arleninov P.D., ?rylov S.B., “Mathematic modeling of Reinforced Concrete Element Operation with cracks under long duration load”, Mathematical and Computer Simulation in Mechanics of Solids and Structures – MCM 2017. Book of Abstracts, 2017, pp. 26-7.

11. GOST 24544-81* “Betony. Metody opredelenija deformacij usadki i polzuchesti State Standart 24544-81*. Concrete. Methods of definition of deformations of shrinkage and creep.,” Moscow, Standartinform Publ., 1987. (In Rusian).

12. Rzhanicyn A.R. “Stroitel'naja mehanika Structural mechanics.”, Moscow, 1982, pp. 251-253 (In Rusian).