Title: High Temperature Effect on Stress-Strain Properties of High-Strength Steel Fiber Concrete

Author(s): Valery Dorf, Rostislav Krasnovsky, Dmitriy Kapustin, and Patimat Sultygova

Publication: Symposium Paper

Volume: 326

Issue:

Appears on pages(s): 65.1-65.10

Keywords: steel fiber concrete, fiber, matrix, stay-in-place forms, high temperature, fire, ultrasonic, tensile bending strength

DOI: 10.14359/51711048

Date: 8/10/2018

Abstract:
The authors of the Report dealing with study of strength and strain characteristics of stay-in-place steel-fiber-reinforced concrete ((SFRC) forms also performing, in process of reinforced concrete structure operation, the functions of load bearing element analyzed the issue of effects of high temperatures occurred during fire on strength of SFRC of the forms and on rate of ultrasound propagation in forms. The results of study may be taken as a basis for development of recommendations for assessment of technical condition of reinforced concrete structures after fire.

Related References:

1. Rabinovich F.N. Fiber reinforced concrete based composites. Theory, design, technology and structures. M. Publisher ACB. 2011. 642 p.

2. Kalashnikov V.I., Tarakanov O.V.; Kuznetsov Y.S., Volodin V.M, Byelyakova E.A. Dry fine-grain powder mix based concrete of new generation // Magazine of Civil Engineering. 2012, ? 8, pp. 47-53.

3. Kaprielov S.S., Karpenko N.I., Sheinfeld A.V., Kuznetsov E.N., Regarding regulation of elastic module and creep of high-strength concrete with MB-50C modifying agent. http://www.master-concrete.com/i/content/reference/66. (2003) doc

4. Pukharenko Y.V?. Scientific and practical bases of formation of fiber-concrete structure and properties. Synopsys of Doctoral thesis. St. Petersburg, 2005, 42 p.

5. Krasnovsky R.O., Dorf V.A. Perspectives of construction of NPP buildings and structures of reinforced concrete blocks with stay-in-place SFRC forms. Construction of nuclear facilities, 2013, No 15, pp.21-27.

6. Dorf V.A., Krasnovsky R.O., Kapustin D.E., Rogachev K.V. Perspectives of development of one of directions of industrialized construction in construction of residential and social buildings. Architecture and construction in Russia. 2012, No 12, pp. 11-15.

7. Kapustin D.E. Stay-in-place SFRC forms as a load bearing element of NPP building and structure reinforced concrete structures. Ph D Thesis in Engineering Science. M. 2016. 282 p.

8. GOST 30247.0-94 Civil structures. Methods of fire resistance testing. General requirements, RF.

9. Guidance for the design of steel-fibre-reinforced concrete // Concrete Society Technical Report 63. 2007, 92 p.

10. Swamy R.N. Fiber Reinforced Cement and Concrete // Proceedings of the Fourth RILEM Internal Symposium. E & FN Spon, (1992).

11. Dhir, Ravindra K. and McCarthy, Michael J. Concrete Durability and Repair Technology. Proceedings of the International Conference. Thomas Telford,

12. Delplace Gilles, Hajar Zi;ul, Simon Alain, Clianut Sandriue, Weizmaun Luc Precast thin UHPFRC curved shells in a waste water treatment plant. . RILEM-fib-AFGC Int. Symposium on Ultra-High Performance Fibre-Reinforced Concrete, UHPFRC 2013 - October 1-3, 2013, Marseille, France, pp.49-58.

13. Nordström Erik Durability of Sprayed Concrete Steel fibre corrosion in cracks, Luleå University of Technology, Sweden, 2005 (Thesis work).

14. Dorf V.A., Krasnovsky R.O., Kapustin D.E., Sultygova P.S. Pozzolanic reaction effects in SFRC high-strength cement-sand matrix at high temperatures. «Bulletin of civil engineers». St. Petersburg ASU. 2017. No 2.

15. Krasnovsky R.O., Rogachev K.V., Denisov A.V. Advantages of use of fiber concrete reinforced by two types of fiber» Materials of Ist International (VIIth All-Russia) NASKR Conference, 2012, Cheboksary.

16. Nekrasov K.D., Zhukov V.V., Gulyayeva V.F. Heavy-weight concrete under increased temperatures. SI. M. 1972, 128 p.

17. Dorf V.A., Krasnovsky R.O., Kapustin D.E., Gorbunov I.A., Nuriyev R.R. Rate of ultrasound propagation in SFRC with cement-sand matrix. Concrete and reinforced concrete. 2014, No 3, pp. 5-8.

18. Demirel Bahar, Kelestemur Oguzhan Effect of elevated temperature on the mechanical properties of concrete produced with finely ground pumice and silica fume. Technical Education Faculty, Construction Department, Firat University, Elazig, 23119, Turkey. Fire Safety Journal 45. 2010, pp. 385–391.

19. Stepanov V.G., Stepanyuchenko V.S. Provision of fire endurance of load bearing reinforced concrete structures. Construction and architecture / Architecture concepts for construction and reconstruction. Togliatti Military Technical Institute. www.rusnauka.com/ 10_NPE_2008/Stroitelstvo/29405.doc.htm

20. Abrams, M.S. Compressive Strength of Concrete at Temperatures to 160 F, Temperature and Concrete. ACI SP-25, pp. 33-58.