Properties of Ultra-High-Strength Self-Compacting Fiber-Reinforced Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Properties of Ultra-High-Strength Self-Compacting Fiber-Reinforced Concrete

Author(s): Simon S. Kaprielov, Andrey V. Sheynfeld, Igor A. Chilin, and Igor M. Bezgodov

Publication: Symposium Paper

Volume: 326

Issue:

Appears on pages(s): 60.1-60.8

Keywords: axial tensile strength; bending tensile strength; compressive strength; creep; elasticity modulus; fiber-reinforced concrete; frost-resistance; ultra-high strength concrete

DOI: 10.14359/51711043

Date: 8/10/2018

Abstract:

It is known that characteristics of fiber-reinforced concrete generally depend on the volume and properties of the matrix, the type and dosage of fiber. Studies have been conducted on the influence of these factors on strength and deformation characteristics, including the modulus of elasticity, creep and frost resistance of ultra-high strength self-compacting fiber reinforced concrete (UHSFRC).

Portland cement CEM I 52.5, sand with fineness modulus of 2.5, organic-mineral modifier MB-50 and straight steel fiber were used as components for self-compacting concrete. The fiber dosage was varied in the range from 0 to 2.0% of the volume of concrete mixtures.

The tests have shown that the creep of steel fiber reinforced concrete at different levels of loading (0.3 and 0.6 of Rb) is significantly less than that of the matrix. The ratio of transverse creep deformation is significantly lower than under the short-time loading, as for the matrix and the same as for steel fiber reinforced concrete. Despite almost linear diagram of concrete deformation under compression, the value of creep deformation shows quite higher figures. It is noted that the effectiveness of steel fiber increases with the increase of stress level.

Freeze-thaw resistance was evaluated in the cyclic process of freezing at -50°C [-58°F] and thawing in 5% NaCl solution. The test results show very high frost resistance of concrete, what corresponds to the grade F2800, what is 2.7 times above the concrete requirements for transport structures in Russia.

Related References:

1. Kaprielov S.S., Sheynfeld A.V., Kardumyan G.S., “New modified concretes”, Printing house “Paradise”, Moscow, 2010, p.258.

2. Ambroise J., Rols S., Pera J., “Properties of self-leveling concrete reinforced by steel fibers. Proceedings of the 3rd International RILEM Workshop on Reinforced Cement Composites”, HPFRCC3, Mainz, 1999, pp.9-17.

3. Kaprielov S.S., Batrakov V.G., Sheynfeld A.V., “Modified concretes of the new generation: reality and perspective”, Concrete and reinforced concrete, No.6, 1999, pp. 6-10.

4. Mishina A.V., Chilin I.A., Andrianov A.A., “Physical and technical properties of ultra-high-performance fiber-reinforced concrete”, Vestnik of MGSU, No.3, 2011, pp. 159-165.

5. The European Guidelines for Self-Compacting Concrete. Specification, Production and Use. BIBM, CEMBUREU, ERMCO, EFCA, EFNARC, May 2005, p.63.

6. Kaprielov S.S., Sheynfeld A.V., Kardumyan G.S., Dondukov V.G., “Modified high-performance fine-grained concretes with improved deformation characteristics”, Concrete and reinforced concrete, No.2, 2006, pp. 2-7.

7. Bondarenko V.M., Yagupov B.A., “The question of calculation of concrete creep”, Journal Academia. Architecture and construction, RAACS, No.3, 2006.

8. Bezgodov I.M. “The question of estimation of the ultimate relative deformation of concrete under compression for different grades of concrete”, Concrete and reinforced concrete, No.5, 2015, pp.9-11.

9. Bezgodov I.M. “The influence of steel fiber on the physical, mechanical and rheological properties of high-strength fine-grained concrete”, Concrete and reinforced concrete, No.1.