Mechanical Properties of Concrete with Recycled Aggregate at Early Ages

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Mechanical Properties of Concrete with Recycled Aggregate at Early Ages

Author(s): Zeger Sierens and Jiabin Li

Publication: Symposium Paper

Volume: 326

Issue:

Appears on pages(s): 39.1-39.10

Keywords: recycled concrete aggregates (RCAs), precast concrete, pre-stressed concrete, strength, modulus of elasticity, early ages

DOI: 10.14359/51711021

Date: 8/10/2018

Abstract:
Currently, recycled concrete aggregates (RCAs) are mainly used in some low-grade applications. New high-value-added applications of this kind of material are required. One possible high-end application is in precast prestressed concrete elements. Knowledge on the mechanical properties of concrete with RCAs at early ages is of crucial importance for this purpose. This paper presents a test program to examine the effect of RCAs on the mechanical properties of concrete at early ages. The main variables in the tests are the percentage of RCAs (0, 10%, 20%, 50% and 100%) and curing age (1d, 2d, 3d, 7d, 14d and 28d). The compressive strength, splitting tensile strength and modulus of elasticity of the concretes are measured. The test results indicate that the use of RCAs tends to decrease the development of the concrete strength and modulus of elasticity with time, but mainly in the first 7 days. The difference increases with the increase of the percentage of RCAs. The test data are also compared with the models in EN 1992-1-1, ACI 209 and ACI 318. It is found that the models can generally provide satisfactory descriptions of the strength and modulus of elasticity of concrete with RCAs at early ages.

Related References:

1. Notermann, B. et al., “Recybet Roadmap – Ontwikkeling van een nieuwe waardeketen voor de valorisatie van betonpuin in betonproducten”, Belgium, 2016.

2. Brandes M.R. and Kurama Y.C., “Use of Recycled Concrete aggregates in Precast/Prestressed Concrete”, Procedia Engineering, Vol.145, 2016, pp. 1338-1345.

3. Soutsos M. N., Tang K. and Millard S. G., “Concrete building blocks made with recycled demolition aggregate”, Construction and Building materials, Vol. 25, No. 2, 2011, pp. 726-735.

4. Tam, V. W. Y., Gao, X., and Tam, C. M., “Microstructural analysis of recycled aggregate concrete produced from two-stage mixing approach”, Cement and Concrete Research, Vol. 35, No. 6, 2005, pp. 1195-1203.

5. Li, J., “Study on mechanical behavior of recycled aggregate concrete”, Master thesis, Tongji University, Shanghai, 2004, 122 pp.

6. EN 1992-1-1: Eurocode 2: Design of concrete structures - Part 1-1: General rules and rules for buildings. Brussels, 2004.

7. ACI Committee 209., “Prediction of creep, shrinkage, and temperature effects in concrete structures”, American Concrete Institute, Farmington Hills, Mich., 2002.

8. ACI Committee 318., “Building code requirements for structural concrete (ACI 318M-14) and commentary (ACI 318RM-14)”, American Concrete Institute, Farmington Hills, Mich., 2014.

9. Xiao, J., Li, J., and Zhang, Ch., “Mechanical properties of recycled aggregate concrete under uniaxial loading”, Cement and Concrete Research, Vol. 35, No. 6, 2005, pp. 1187-1194.

10. Xiao, J., Li, J., and Zhang, Ch., “On relationships between the mechanical properties of recycled aggregate concrete: an overview”, Materials and Structures, Vol. 39, No. 6, 2006, pp. 655-664.