Title: Contribution to the study of failure behaviour of the vertical joints between big concrete panels

Author(s): Catalá Alis, J.; Moragues Terrades, J. J.; Miguel Sosa, P.

Publication: ACHE

Volume: 36

Issue: 154

Appears on pages(s): 191 -

Keywords:

DOI:

Date: 1/1/1985

Abstract:


ACI International Partner, ACHE Spain, International Partner Access