Some thoughts on the dynamic modeling of bridges

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Some thoughts on the dynamic modeling of bridges

Author(s): Casas Rius, J.R.

Publication: ACHE

Volume: 45

Issue: 191

Appears on pages(s): 127 - 136

Keywords:

DOI:

Date: 1/3/1994

Abstract:
Because of the highly different bridge types and designs used in bridge engineering which derive on largely different dynamic mechanisms of response, one of the most important problems to solve concerning their theoretical dynamic modelling is to choose the most adequate FEM model for a particular bridge. The paper deals with the work carried out related with dynamic testing of several bridges in order to check the feasibility and accuracy of different finite element analytical models assumed for the dynamic behaviour of different bridge types: continuous prestressed concrete box girder bridges, continuous prestressed slab bridges with small and large width sections, cable-stayed bridges, etc. The experimental data coming from the tests is used to derive the real dynamic properties of the bridge (natural frequencies and mode shapes). The most appropiate and simple analytical models and dynamic properties of the elements to be used in the FEM mesh are derived for each bridge type based on correlation between theoretical and experimental results. Taking into account these results a set of practical recommendations for the dynamic modelling of different bridges is derived.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »  



  