Metlac bridge in Mexico

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Metlac bridge in Mexico

Author(s): Fernández Troyano, L.; Manterola Armisén, J.

Publication: ACHE

Volume: 42

Issue: 180

Appears on pages(s): 99 - 107

Keywords:

DOI:

Date: 1/5/1991

Abstract:
The Metlac viaduct for the Mexico-Veracruz railroad is built over a 120 m deep gorge and it has a 90 m log maximum span. It supports a double track with 6,5 m depth and 10 m width. The whole morphology of the structure and the supports has been defined on the basis of the high seismic risk on the area. The continuous beam is cut in two parts with a central double hionged beam to allow for larger displacements since the gorge may be due to and active fault. Each half of the bridge is built into the abutments, which are connected to the ground through prestressed anchorages.


ACI International Partner, ACHE Spain, International Partner Access

View Resource »