Hybrid beam of 8 meters length manufactured with concrete and composites materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Hybrid beam of 8 meters length manufactured with concrete and composites materials

Author(s): Mieres Royo, J.M.; Bautista Carrascosa, S.; Calvo Herrera, I.

Publication: ACHE

Volume: 54

Issue: 230

Appears on pages(s): 71 - 79

Keywords:

DOI:

Date: 1/8/2003

Abstract:
The project theme is the development of an all-in-one composite reinforcing formwork system that could eventually substitute the standard materials used for making reinforced concrete elements like steel. The concept consists in substituting the standard steel or wooden formwork, usually used to manufacture reinforced concrete structures, with an FRC formwork. The FRC formwork would not (as is normally the case) be dismantled once the concrete was set, but rather would be bonded to the concrete; thus acting as tensile reinforcement in substitution of the usual steel reinforcement bars and stirrups. The key engineering concepts to be examined were: ? Structural failure modes ? Creep and relaxation characteristics ? Optimization of overall stiffness by proper use of material properties ? Monitoring of structural performance, particularly the bonded concrete-composite interface using optical fibre techniques.


ACI International Partner, ACHE Spain, International Partner Access