The economic use of advanced polymer composites with concrete in structures (COMPCON R&D BRITE project)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The economic use of advanced polymer composites with concrete in structures (COMPCON R&D BRITE project)

Author(s): Hué García, F.

Publication: ACHE

Volume: 55

Issue: 234

Appears on pages(s): 109 - 119

Keywords:

DOI:

Date: 1/8/2004

Abstract:
This paper describes the R&D Project COMPCON carried on with european financial help. During 3.5 years the economic applications in structures of composites with concrete were studied. Composites offer various advantages, lightweight and long durability, but we need to better understand how it can be applied in building and civil engineering construction. A long span beam comprising a concrete top slab (compression) located within a GFRP permanent shutter and a hollow box shell beneath (shear and tensile) of CFRP+GFRP composite was developed. The viability of this structural solution and other concrete+composites combinations for efficient, durable and cost-effective construction were studied. It was shown that these beams could be simply and effectively manufactured using ?prepreg? composites, fresh resin factory pre-impregnated, manufactured in rolled thin sheets. It is applied on a free form mould in consecutive layers and then curing it in place under vacuum and moderated temperature (65ºC), suitable for construction site conditions.