Title: Effects of Silica Fume Content and Polymer-Binder Ratio on Properties of Ultrarapid-Hardening Polymer-Modified Mortars

Author(s): Jong Yun Choi, Myung-Ki Joo, and Byeong Cheol Lho

Publication: IJCSM

Volume: 10

Issue: 2

Appears on pages(s): 249–256

Keywords: polymer-modified mortar, polymer-binder ratio, silica fume content, strength, water absorption, carbonation depth, chloride ion penetration depth.

DOI: 10.1007/s40069-016-0136-9

Date: 6/30/2016

Abstract:
This paper deals with the effects of silica fume content and polymer-binder ratio on the properties of ultrarapidhardeningpolymer-modified mortar using silica fume and ethylene-vinyl acetate redispersible polymer powder instead of styrenebutadienerubber latex to shorten the hardening time. The ultrarapid-hardening polymer-modified mortar was prepared with varioussilica fume contents and polymer-binder ratios, and tested flexural strength, compressive strength, water absorption, carbonationdepth and chloride ion penetration depth. As results, the flexural, compressive and adhesion strengths of the ultrarapid-hardeningpolymer-modified mortar tended to increase as increasing polymer-binder ratio, and reached the maximums at 4 % of silica fumecontent. The water absorption, carbonation and chloride ion penetration resistance were improved according to silica fume contentand polymer-binder ratio.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer