Title: High Magnitude Loading of Concrete Bridges

Author(s): Jacob W. Schmidt, Philip S. Halding, Thomas W. Jensen, Svend Engelund

Publication: Symposium Paper

Volume: 323

Issue:

Appears on pages(s): 9.1-9.20

Keywords: Full-scale testing, concrete bridges, test rig, advanced monitoring, Danish standard vehicles, structural response, modelling

DOI: 10.14359/51702439

Date: 5/1/2018

Abstract:
The motivation for full-scale testing of concrete bridges is significant, since it is deemed to solve some of the major challenges related to capacity evaluation of older concrete bridges combined with increasing load demands. A novel test rig was developed as a mean to evaluate the full-scale bridge response of concrete bridges spanning up to 12 m (39.4 feet). The test rig was fast to mount, applied the load accurately, and loaded the structures to a very high load magnitude. The bridges were loaded to maximum capacity of the test rig without cracking (approx. 100 tonne (220,000 lbs) axle loads). 3D scanning, LVDTs, distance lasers, and DIC cameras were applied to two of the bridges, as well as land surveying readings, in order to measure the structural behaviour during testing. The loading sequence worked well, and it was possible to measure deflections and strains. Using a wide-angle lens DIC-camera showed to be a promising method to measure strains, in-plane deformations and cracking during testing. Work regarding modelling in conjunction with monitoring is ongoing, to provide a more accurate way to evaluate the ultimate capacity of the bridges as well as stop criteria during full-scale testing.

Related References:

Danish Road Directorate, EN 1991-2 DK NA:2009 - Annex A – Lastmodeller for klassificering og bæreevnevurdering, 2009.

Danish Road Directorate, 978-87-7060-359-1 – Broer. Vejledning til belastnings- og beregningsgrundlag, 2010.

Alkhrdaji, T.; Barker, M.; Chen, G.; Mu, H.; Nanni, A. and Yang, X., 2001, "Destructive and non-destructive testing of bridge J857, Phelps County, Missouri. Volume 1 - strengthening and testing to failure of bridge decks"

Azizinamini, A., 1994, "Old concrete slab bridges.1. Experimental investigations", Journal of Structural Engineering-Asce, V. 120, No. 11.

Bergström, M.; Täljsten, B. and Carolin, A., 2009, "Failure Load Test of a CFRP Strengthened Railway Bridge in Örnsköldsvik, Sweden", Journal of Bridge Engineering, V. 14, No. 5, pp. 300–308. doi: 10.1061/(ASCE)BE.1943-5592.0000005

Canon Global, www.canon.com (accessed June 14, 2017)

Elmont, V. J., 1913, "Test-loading until breaking point of a 100-foot arch bridge", Canadian Engineer.

EnerPac, www.enerpac.com (accessed June 14, 2017)

GOM, www.gom.com (accessed June 14, 2017)

Goodpasture, D. W. and Burdette, E. G., 1973, "Full Scale Tests to Failure of Four Highway Bridges", American Railway Engineering Association, V. 74, No. 643, pp. 454–473.

Gosbell, K. B. and Stevens, L. K., 1968, "Test loading of a full scale bridge", In A.R.R.B Proceedings, V. 4, pp. 2018–2041.

HBM, www.hbm.com (accessed June 14, 2017)

Isaksen, H. R.; Kanstad, T. and Olsen, P.-E., 1998, "Prøvebelastning av bru nr 02-1234 Smedstua bru.

Jorgenson, J. L. and Larson, W., 1976, "Field Testing of a Reinforced Concrete Highway Bridge to Collapse, Transportation Research Record, No. 607, pp. 66–71.

Köppel, S. and Vogel, T., 1997, "Feldversuch Steilerbachbrücke", doi: 10.3929/ETHZ-A-001853810

Lantsoght, E. O. L., 2013, "Shear In Reinforced Concrete Slabs under Concentrated Loads close to Supports", doi: 10.4233/UUID:3C0045DC-66B2-4151-B778-C318A96B22BC

Leuze electronic, www.leuze.com (accessed June 14, 2017)

Matterport, www.matterport.com (accessed June 14, 2017)

Nanni, A.; Alkhrdaji, T.; Chen, G.; Barker, M.; Yang, X. and Mayo, R., 1999, "Overview of testing to failure of a highway bridge strengthened with FRP composites", In 4th International Symposium on FRP for Reinforcement of Concrete Structures (FRPRCS4), pp. 69–80.

Novotechnik, www.novotechnik.com. (accessed June 14, 2017)

Pedersen, E. S.; Nielsen, P. M. and Lyngberg, B. S., 1980, "Investigation and failure test of a prestressed concrete bridge". In 11th Congress - International Association for Bridge and Structural Engineering (iabse) Final Report, pp. 849–854.

Plos, M., 1995, "Application of fracture mechanics to concrete bridges", Chalmers tekniska ho¨gskola. Avdelningen fo¨r betongbyggnad.

Rösli, A., 1963, "Die Versuche an der Glattbrücke in Opfikon", Eidgenössische Materialprüfungs- Und Versuchsanstalt Für Industrie, Bauwesen Und Gewerbe, V. 192, No. 85.

Schmidt, J. W.; Hansen, S. G.; Barbosa, R. A. and Henriksen, A., 2014, "Novel shear capacity testing of ASR damaged full scale concrete bridge", Engineering Structures, V. 79, pp. 365–374. doi: 10.1016/j.engstruct.2014.08.027

Song, H.-W.; You, D.-W.; Byun, K.-J. and Maekawa, K., 2002, "Finite element failure analysis of reinforced concrete T-girder bridges", Engineering Structures, V. 24, No. 2, pp. 151–162. doi: 10.1016/S0141-0296(01)00107-9

Unknown, 1952, "Destruction of the Prestressed Concrete Footbridge at the South Bank", Civil Engineers Review, V. 6, No. 8, pp. 330–334.

Zhang, J.; Peng, H. and Cai, C. S., 2011, "Field Study of Overload Behavior of an Existing Reinforced Concrete Bridge under Simulated Vehicle Loads", Journal of Bridge Engineering, V. 16, No. 2, pp. 226–237. doi: 10.1061/(ASCE)BE.1943-5592.0000140

Zhang, J.; Peng, H. and Cai, C. S., 2013, "Destructive Testing of a Decommissioned Reinforced Concrete Bridge", Journal of Bridge Engineering. V. 18, No. 6, pp. 564–569. doi: 10.1061/(ASCE)BE.1943-5592.0000408