Title: Influence of Applied Loads on the Permeability Behavior of Ultra High Performance Concrete with Steel Fibers

Author(s): Zhiming Ma, Tiejun Zhao, Xiaochuan Yao

Publication: JCI

Volume: 14

Issue: 12

Appears on pages(s): 770 - 781

Keywords:

DOI: 10.3151/jact.14.770

Date: 1/1/2016