Title: Shear Strength of Reinforced Concrete Beams: Concrete Volumetric Change Effects

Author(s): Kenichiro Nakarai, Shigemitsu Morito, Masaki Ehara, Shota Matsushita

Publication: JCI

Volume: 14

Issue: 5

Appears on pages(s): 229 - 244

Keywords:

DOI: 10.3151/jact.14.229

Date: 1/1/2016