Title: Cracking and Chemical Composition of Cement Paste Subjected to Heating and Water Re-Curing

Author(s): Michael Henry, Katsufumi Hashimoto, Ivan Sandi Darma, Takafumi Sugiyama

Publication: JCI

Volume: 14

Issue: 4

Appears on pages(s): 134 - 143

Keywords:

DOI: 10.3151/jact.14.134

Date: 1/1/2016