Title: Application of Electrodeposition Method in Upgrading Mortar Durability

Author(s): Jinxia Xu, Wei Feng, Hongyou Shan, Linhua Jiang, Li Tang

Publication: JCI

Volume: 13

Issue: 7

Appears on pages(s): 367 - 372

Keywords:

DOI: 10.3151/jact.13.367

Date: 1/1/2015

Abstract:


Japan Concrete Institute, International Partner Access