Title: Ultrasonic Nondestructive Testing of Cement Grouting Quality in Corrugated Pipes Based on Impact-echo

Author(s): Qingbang Han, Jin Cheng, Honghui Fan, Cheng Yin, Changping Zhu

Publication: JCI

Volume: 12

Issue: 11

Appears on pages(s): 503 - 509

Keywords:

DOI: 10.3151/jact.12.503

Date: 1/1/2014