Title: Behavioral Simulation Model for SFRC and Application to Flexural Fatigue in Tension

Author(s): Xuejuan Tang, Xuehui An, Koichi Maekawa

Publication: JCI

Volume: 12

Issue: 10

Appears on pages(s): 352 - 362

Keywords:

DOI: 10.3151/jact.12.352

Date: 1/1/2014

Abstract:


Japan Concrete Institute, International Partner Access