Title: Durability of Recycled Aggregate Concrete: An Overview
Author(s): Jianzhuang Xiao, Deng Lu, Jingwei Ying
Publication: JCI
Volume: 11
Issue: 12
Appears on pages(s): 347 - 359
Keywords:
DOI: 10.3151/jact.11.347
Date: 1/1/2013
Abstract: