Title: Strength Targeted PBMD of HSC based on One-parameter Bayesian Probabilistic Method

Author(s): Hung Duc Phan, Jang-Ho Jay Kim, Na-Hyun Yi, Young-Jun You, Jong-Wook Kim

Publication: JCI

Volume: 10

Issue: 4

Appears on pages(s): 137 - 150

Keywords:

DOI: 10.3151/jact.10.137

Date: 1/1/2012

Abstract:


Japan Concrete Institute, International Partner Access

View Resource »  



  