Title:
Steel Corrosion Induced by Chloride or Carbonation in Mortar with Bending Cracks or Joints
Author(s):
Shin-ichi Miyazato, Nobuaki Otsuki
Publication:
JCI
Volume:
8
Issue:
2
Appears on pages(s):
135 - 144
Keywords:
DOI:
10.3151/jact.8.135
Date:
1/1/2010