Title: Experimental Study on Bond-Strengthening Hooks for RC Beams

Author(s): Yuichi Sato, Katsuhiro Nagatomo, Yoshifumi Nakamura

Publication: JCI

Volume: 7

Issue: 2

Appears on pages(s): 263 - 271

Keywords:

DOI: 10.3151/jact.7.263

Date: 1/1/2009

Abstract:


Japan Concrete Institute, International Partner Access