Title: Simplified Inverse Method for Determining the Tensile Properties of Strain Hardening Cementitious Composites (SHCC)

Author(s): Shunzhi Qian, Victor C. Li

Publication: JCI

Volume: 6

Issue: 2

Appears on pages(s): 353 - 363

Keywords:

DOI: 10.3151/jact.6.353

Date: 1/1/2008