Title: Simulation of Chloride Diffusivity for Cracked Concrete Based on RBSM and Truss Network Model

Author(s): Licheng Wang, Mitsutaka Soda, Tamon Ueda

Publication: JCI

Volume: 6

Issue: 1

Appears on pages(s): 143 - 155

Keywords:

DOI: 10.3151/jact.6.143

Date: 1/1/2008

Abstract: