Title: Strength and Ductility of Non-Embedded Steel Reinforced Concrete Column Base

Author(s): Ryoichi Shohara, Yoshikazu Sawamoto, Kazumasa Imai, Haruo Nakazawa, Hiroyuki Narihara, Toshiyuki Fukumoto

Publication: JCI

Volume: 5

Issue: 2

Appears on pages(s): 223 - 234

Keywords:

DOI: 10.3151/jact.5.223

Date: 1/1/2007

Abstract:


Japan Concrete Institute, International Partner Access