Title: Modeling of Calcium Leaching from Cement Hydrates Coupled with Micro-Pore Formation

Author(s): Kenichiro Nakarai, Tetsuya Ishida, Koichi Maekawa

Publication: JCI

Volume: 4

Issue: 3

Appears on pages(s): 395 - 407

Keywords:

DOI: 10.3151/jact.4.395

Date: 1/1/2006