Title: Tensile and Anti-Spalling Properties of Direct Sprayed ECC

Author(s): Tetsushi Kanda, Tadashi Saito, Noboru Sakata, Masanori Hiraishi

Publication: JCI

Volume: 1

Issue: 3

Appears on pages(s): 269 - 282

Keywords:

DOI: 10.3151/jact.1.269

Date: 1/1/2003