Abstract:
This series of sessions, co-organized by fib, serves as an interim to the Bond in Concrete conference series, held in Europe every 10 years. Various presentations will highlight the following information: 1) important changes required to development and lap splice provisions for reinforcement; 2) new works and developments as related to the modelling of bond between reinforcing steel and concrete; and 3) the results of recent experimental studies relating to lap splicing of straight bars.