Title: Use of Stockpile and Lagoon Ashes for the Manufacture of Aerated Concrete Blocks

Author(s): Robert Carroll

Publication: Institute of Concrete Technology

Volume:

Issue:

Appears on pages(s): 4 pages

Keywords:

DOI:

Date: 1/1/2017

Abstract:
Fly ash derived from coal-fired power stations is the major silica source used for the manufacture of autoclaved aerated concrete (AAC) in the United Kingdom. Typically between 500 000 and 750 000 tonnes of the by-product are used each year. The technical and environmental benefits associated with the use of fly ash contribute to achieving sustainable construction products. This papers briefly reviews the history of the use of fly ash for the manufacture of AAC in the United and discusses the processing methods and relevant specifications. Sources and potential constraints on fly ash supply are noted, as are the on-going efforts to develop complementary sources. Of particular importance for the future manufacture of AAC are the challenges and opportunities of using stockpile and lagoon ashes.


Institute of Concrete Technology, International Partner Access

View Resource »  



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer