Title: ACI Concrete Sustainability Forum VIII

Author(s): Koji Sakai and Julie K. Buffenbarger

Publication: Concrete International

Volume: 38

Issue: 4

Appears on pages(s): 72-76

Keywords: prestressed, cement, carbon, building

DOI:

Date: 4/1/2016

Abstract:
The Concrete Sustainability Forum VIII was held in Denver, CO, at The ACI Concrete Convention and Exposition – Fall 2015. The forum included presentations by seven speakers, panel discussions between speakers and audience, and a tour of the National Renewable Energy Laboratory. The presentations, discussions, and tour are summarized.




  