International Concrete Abstracts Portal

  


Title: Numerical Simulation of BFRP Confined Reinforced Concrete Columns

Author(s): Zhiwen Xiong and Yongsheng Liu

Publication: China Concrete and Cement Products

Volume:

Issue: No.4 2010(Total 174)

Appears on pages(s): 42-44

Keywords: BFRP, Reinforced concrete square columns, Numerical simulation, Crack

DOI:

Date: 8/20/2010

Abstract:
The process of axial compression of the basalt fiber (BFRP) confined reinforced concrete columns is simulated by using ANSYS software,and the stress distribution and crack development of basalt fiber (BFRP) confined concrete columns are obtained,which are compared and analyzed with the test results.The results show that the discrete model for finite element numerical analysis can simulate the axial loaded behavior of BFRP confined concrete columns.Based on simulation results,the force analysis of the failure process of BFRP confined reinforced concrete square columns is taken and the interaction mechanism between BFRP cloth and concrete under axial compression is discussed.
To order a copy of this publication EMail CCPA at Qinghuan Zhang


China Concrete and Cement Products, International Partner Access

View Resource »  



  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer