Future Trends in Roller Compacted Concrete Dam Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Future Trends in Roller Compacted Concrete Dam Construction

Author(s): M. R. H. Dunston

Publication: Symposium Paper

Volume: 144

Issue:

Appears on pages(s): 307-324

Keywords: arch dams; blast furnace slag; construction; dams; fly ash; gravity dams; mix proportioning; pozzolans; roller compacted concrete; Construction

DOI: 10.14359/4505

Date: 3/1/1994

Abstract:
Roller compacted concrete (RCC) became an accepted method for dam construction during the latter half of the 1980s and during the early 1990s there has been a very rapid growth in this form of dam. High dams up to 200 m in height and containing several million m 3 of concrete are now being designed. Paper describes the development of RCC dams over the last decade and shows how there has been a move away from the early RCC dams that contained a relatively low cementitious content toward a dam that contains higher cementitious contents, usually with a high proportion of pozzolan. Although a number of different pozzolans have been used, the significant majority of RCC dams have contained low-lime fly ash. The in-situ properties that have been achieved in RCC dams already in service for a number of years have been found to be suitable for gravity dams more than 200 m high. Arch-gravity RCC dams have been completed with heights approaching 80 m, together with a thick-arch RCC dam of a comparable height. It is considered that the traditional concrete dam will be superseded within the not-too-distant future by the RCC method of construction, and on a number of sites where rock-fill dams were originally planned, RCC dams will eventually be constructed.