Construction of a Dry Dock Using Tremie Superplasticized Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Construction of a Dry Dock Using Tremie Superplasticized Concrete

Author(s): M. Collepardi, R. Khurana, and M. Valente

Publication: Symposium Paper

Volume: 119

Issue:

Appears on pages(s): 471-492

Keywords: concrete construction; concrete slabs; drydocks; permeability; plasticizers; sulfate resistance; tremie concrete; workability; Materials Research

DOI: 10.14359/2548

Date: 9/1/1989

Abstract:
Describes the construction of San Marco dry dock in Italy. Approximately 82,000 m3 of superplasticized concrete with a slump of 250 mm was placed, of which 40,000 m3 were underwater at a depth of 16 m using a tremie system. The concrete was mixed at a central plant and transported to the site where it was pumped for 250 m from a fixed station to the hopper of the tremie located on a floating barge. The presence of heavy reinforcement (steel trestles) made the positioning of the tremie pipe and inspection by divers very difficult. To limit the number of shiftings of the tremie pipe, concrete had to have a very high workability and had to be very cohesive to prevent washing by seawater. Moreover, the specification required an impermeable, sulfate-resistant concrete with a strength of 25 MPa. In the first stage, a slab of 4 m thickness was created by placing overlapping "pizzas" of 45 m3 volume and 15 m diameter. If the concrete was not superplasticized, then the size of the "pizzas" would have been much smaller (approximately 20 m3 volume and 3 to 4 m diameter). After dewatering, the slab was completed with a second pour of self-levelling concrete of 1 m thickness. The use of a superplasticizer helped the contractor complete the job 3 months ahead of schedule.




  