Title:
Strengthening of RC Structures with Textile Reinforced Concrete (TRC)
Author(s):
S. Weiland, R. Ortlepp, A. Bruckner, and M. Curbach
Publication:
Symposium Paper
Volume:
244
Issue:
Appears on pages(s):
157-172
Keywords:
fiber; reinforced concrete; retrofitting; strengthening; textile; textile reinforced concrete (TRC); TRC application
DOI:
10.14359/18758
Date:
5/1/2007
Abstract:
Strengthening by textile reinforced concrete noticeably increases both the ultimate load bearing capacity as well as the serviceability - especially deflections, crack widths and crack spacing are reduced. Beside that there are still some practical applications. This paper will give an overview of the ongoing research work with this new composite material Textile Reinforced Concrete (TRC).