Title: Displacement versus Force-Seeking Effects for Reinforced Concrete Frames

Author(s): G.C. Ernst and G.M. Smith

Publication: Symposium Paper

Volume: 53

Issue:

Appears on pages(s): 227-246

Keywords: dynamic structural analysis; earthquake resistant structures; earthquakes; failure; frames; lateral pressure; live loads; loads (forces); oscillations; plastic analysis; reinforced concrete; static loads; structural analysis

DOI: 10.14359/17699

Date: 1/1/1977

Abstract:
Oscillatory motions were applied to continuous reinforced concrete frames under laboratory control for both displacement and forces seeking conditions.




  