Title: Influence of Temperature on the Creep of Mass Concrete

Author(s): Antonio Ferreira Da Silveria and Carlos Alberto Florentino

Publication: Symposium Paper

Volume: 25

Issue:

Appears on pages(s): 173-190

Keywords: age; creep properties; creep recovery; dams; mass concrete; plain concrete; strains; stress-strain relationships; temperature; water-cement ratio

DOI: 10.14359/17336

Date: 1/1/1971

Abstract:
The present paper describes the results of creep tests carried out at LNEC on two kinds of mass cured concrete; the constant load being applied at different ages (3 to 365 days) and at two test temperatures: room temperature and 45 C.




  