Abstract:
There has been a very marked change, during the last few years, in preparing materials for concrete purposes. We seldom see the old obsolete method of sending a team to a river bank, or put for gravel aggregate, regardless of size, proportion or cleanliness. We now see a modern factory for handling, sizing and washing the gravel that decreases the cost of handling, prepares it for different kinds of uses, and, best of all, makes it suitable for the purpose.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer