The Middleboro, Mass., Reinforced Cocnrete Water Tower Tank

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Middleboro, Mass., Reinforced Cocnrete Water Tower Tank

Author(s): G.A. Sampson

Publication: Journal Proceedings

Volume: 12

Issue: 2

Appears on pages(s): 51-58

Keywords: none

DOI: 10.14359/15978

Date: 2/1/1916

Abstract:
The history of reinforced concrete standpipes and elevated tanks for storage of water had its origin in this country at Mildford, Ohio, in 1903. The first structure was a standpipe having a capacity of 93,000 gal. with an inside diameter of 14 ft. and a depth of water of 78ft. Although the development in this branch of concrete construction has been somewhat slow in the thirteen years elapsed, and marked with a few doubtful successes, there are nevertheless a considerable number now in use that have proven the adaptability and advantages of concrete for these types of structures.




  

Edit Module Settings to define Page Content Reviewer