Title: Flexural Strength of Plain Concrete
Author(s): Duff A. Abrams
Publication: Journal Proceedings
Volume: 18
Issue: 2
Appears on pages(s): 20-45
Keywords:
DOI: 10.14359/15670
Date: 2/1/1922
Abstract: The flexural strength of concrete is low as compared with its compressive stregth; the use of steel bars to supply this deficiency is the basic prinicple of reinforced concrete construction.