Notes on a Severe Formwork Fire

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Notes on a Severe Formwork Fire

Author(s): Arthur R. Lord

Publication: Journal Proceedings

Volume: 19

Issue: 1

Appears on pages(s): 27-38

Keywords: none

DOI: 10.14359/15630

Date: 1/1/1923

Abstract:
Within the memory of the youngest of us the construction of concrete buildings halted at the approch of winter.