Title: SP-137: Polymer Concrete

Author(s): Editor: D. Gerry Walters

Publication: Symposium Paper

Volume: 137

Issue:

Appears on pages(s): 130

Keywords:

DOI: 10.14359/14177

Date: 6/1/1993

Abstract:
SP-137 An ACI publication providing information on an assortment of polymer concrete-related topics. Polymers are gaining increasing use in concrete due to the fantastic properties that they can provide. Polymer concrete is used for repairs, bridge deck and floor overlays, precast products, and structural members. Other uses are continuously under development.




  