Realizing The Potential Of Concrete As A Construction

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Realizing The Potential Of Concrete As A Construction

Author(s): Bryant Mather

Publication: Symposium Paper

Volume: 223

Issue:

Appears on pages(s): 11-19

Keywords: Concrete; Durability; Environment; Ethics; Service life; Specification overkill; Statistical methods; Uniformity; Variability

DOI: 10.14359/13493

Date: 10/1/2004

Abstract:
Concrete is international, but made locally; has infinite variability, but can be made very uniform; and can be made to last as long as you want it to. Therefore, what is needed to more fully realize its potential as a construction material is to understand what we want it to do, learn how to make it so it will do so, use available methods to restrict undesired variability, consider the ethical and environmental aspects of its use, and help the people who are making it to do it better.